Includes bibliographical references (p. 362) and index.
یادداشتهای مربوط به مندرجات
متن يادداشت
Cover; Half-title; Title; Copyright; Contents; Foreword; Preface; Acknowledgements; 1 Introduction; 2 The physical metallurgy of nickel and its alloys; 3 Single-crystal superalloys for blade applications; 4 Superalloys for turbine disc applications; 5 Environmental degradation: the role of coatings; 6 Summary and future trends; Index;
بدون عنوان
0
یادداشتهای مربوط به خلاصه یا چکیده
متن يادداشت
Superalloys are unique high temperature materials used in gas turbine engines, which display excellent resistance to mechanical and chemical degradation. This book introduces the metallurgical principles which have guided their development. Suitable for graduate students and researchers, it includes exercises and additional resources at www.cambridge.org/9780521859042.
ویراست دیگر از اثر در قالب دیگر رسانه
عنوان
Superalloys.
شماره استاندارد بين المللي کتاب و موسيقي
9780521859042
موضوع (اسم عام یاعبارت اسمی عام)
موضوع مستند نشده
Heat resistant alloys.
موضوع مستند نشده
TECHNOLOGY & ENGINEERING-- Material Science.