بررسی آزمایشگاهی تزریق ژل به منظور جلوگیری از تولید آب اضافی در چاههای نفتی
General Material Designation
[پایاننامه]
Parallel Title Proper
Experimental investigation of gel injection to prevent excessive water production in oil wells
First Statement of Responsibility
/محمد صابر دبیری
.PUBLICATION, DISTRIBUTION, ETC
Name of Publisher, Distributor, etc.
: مهندسی نفت و گاز
Date of Publication, Distribution, etc.
، ۱۳۹۸
PHYSICAL DESCRIPTION
Specific Material Designation and Extent of Item
۱۲۰ص.
Other Physical Details
:
GENERAL NOTES
Text of Note
زبان: فارسی
Text of Note
زبان چکیده: فارسی
NOTES PERTAINING TO PUBLICATION, DISTRIBUTION, ETC.
Text of Note
چاپی - الکترونیکی
NOTES PERTAINING TO PHYSICAL DESCRIPTION
Text of Note
مصور، جدول، نمودار
DISSERTATION (THESIS) NOTE
Dissertation or thesis details and type of degree
کارشناسی ارشد
Discipline of degree
مهندسی نفت- بهرهبرداری
Date of degree
۱۳۹۸/۱۱/۰۱
Body granting the degree
صنعتی سهند
SUMMARY OR ABSTRACT
Text of Note
امروزه از ژلهای پلیمری به منظور مقابله با مشکل تولید آب استفاده میشود .در این پژوهش تاثیر پارامترهای مختلف بر روی خواص ژل پلیآکریلآمید/استات(III) کروم با استفاده از آزمایش بطری و سیلابزنی مورد ارزیابی قرار گرفت .با استفاده از آزمایش بطری ژل در غلظتهای مختلف پلیمر و نسبتهای گوناگون عامل شبکهکنندهای به پلیمر بررسی شد .با استفاده از نتایج آزمایشهای بطری ژل بهینه با غلظت بهینهppm ۱۰۰۰۰ پلیمر و نسبت عامل شبکهکنندهای ۴۰:۱ تعیین شد .در ادامه تاثیر پارامترهای مختلف بر روی زمان ژل شدن بررسی شد .حضور نمکهای تک و دو ظرفیتی باعث کاهش استحکام و زمان ژل شدن میشود که در این میان تاثیر یونهای دو ظرفیتی بیشتر از نمکهای تک ظرفیتی است .نتایج آزمایش بطری نشان داد که در غلظتهای پایین تر از ppm ۱۰۰۰ کلرید سدیم نرخ ژل شدن افزایش پیدا میکند یعنی مدت زمان بیشتری طول میکشد تا محلول ژلانت در دمای ۸۰ درجه سانتیگراد تبدیل به ژل شود .در همه غلظتهای بررسی شده ژل مورد نظر بعد از گذشت مدت زمان ۵۱ ساعت به درجه استحکام G رسیده است و درنهایت بعد از گذشت ۷۹ ساعت به درجه استحکام I رسیده است .به طور کلی میتوان نتیجه گرفت که غلظت این یون بر روی محلول ژلانت ساخته شده با درصد وزنی ۰/۱ پلیمر و ۰/۰۲۵ استات کروم تأثیر اندکی دارد .بنابراین این محلول ژلانت گزینه مناسبی برای انجام آزمایشهای سیلابزنی میتواند باشد .همچنین نتایج تست بطری نشان داد که میزان مقاومت ژل با افزایش pH محلول پلیمری به بالای ۷، افزایش پیدا میکند .با توجه به آزمایش میزان ژل شدن توسط محیط قلیایی کنترل میشود و نشان میدهد که نرخ میزان ژل شدن در محیطهای اسیدی به تأخیر میافتد و همچنین مقاومت ژل در pH اسیدی کاهش پیدا میکند.
Text of Note
C. In all concentrations studied, the desired gel reached the degree of G strength after 51 hours and finally reached the strength of I after 79 hours. In general, it can be concluded that the concentration of this ion has little effect on the gelatin solution made with the weight percentage of 0.1 polymer and 0.25 chromium acetate. Therefore, this gelatin solution can be a good option for flooding experiments. Also, the results of the bottle test showed that the resistance of the gel increases with increasing the pH of the polymer solution to above 7. According to the test, the amount of gelling is controlled by the alkaline medium and shows that the rate of gelling is delayed in acidic environments and also the resistance of the gel to acidic pH is reduced. In order to evaluate the gel in the porous media, 5 flooding experiments were designed. The first experiment was performed as a basis and only with the flooding process with water. The second experiment was performed to evaluate the performance of the gel in reducing water production and increasing oil recovery. The third and fourth experiments were performed to investigate the effect of salinity on gel performance and the fifth experiment was performed to evaluate the effect of pH. The results of flooding experiments showed that increasing the salinity will reduce the performance of the gel, so that in flooding with salt water with a concentration of 165000 ppm water production will be reduced to a lesser extent and will reduce the efficiency of the gel. Also, the results of flooding test showed that the gel has a better performance in high pH and alkaline environments, so that in the fifth experiment, which was performed in acidic pH, the water production decreased compared to the third and fourth experiments, which were performed in alkaline environment, was less. ░ nowadays, polymer gels are used to combat water production. In this study, the effect of different parameters on the properties of HPAM/Cr3+ gel was evaluated using bottle testing and flooding. Using gel bottle testing in different concentrations of polymer and different ratios of crosslinking agent to polymer were investigated. Using the results of experiments of bottle test, the optimal gel with a concentration of 10,000 ppm polymers and a crosslinking agent ratio 1:40 was determined. Then, the effect of different parameters on the gelling time was investigated. The presence of monovalent and divalent salts reduces the strength and gelling time, in which the effect of divalent ions is more than monovalent salts. The results of the bottle test showed that at concentrations below 1000 ppm sodium chloride the rate of gelation increased, it took longer for the gelatin solution to gel at 80
ba
PARALLEL TITLE PROPER
Parallel Title
Experimental investigation of gel injection to prevent excessive water production in oil wells
TOPICAL NAME USED AS SUBJECT
کنترل تولید آب
ژل پلیمر
برش آب
UNCONTROLLED SUBJECT TERMS
Subject Term
Control of water production; Gel Polymer; Water cut